Retort processing exposes packaging to the most aggressive thermal and moisture environment in food manufacturing. A film that passes shelf-life testing at ambient temperature can still fail in an autoclave, and the failure usually appears as delamination.

What heat does to EVOH

At elevated temperature the barrier layer absorbs moisture faster and the crystallinity drops, so the OTR climbs. The film does not decompose at 121 °C, but its barrier performance during and immediately after the cycle is materially worse than at ambient. A retort-grade structure is therefore designed with a margin, not to the threshold.

Why delamination happens

Delamination in retort packs is an adhesive problem, not an EVOH problem. Solvent-based laminations fail because the adhesive cannot survive steam at temperature. Coextruded tie layers bonded under heat and pressure do not have this failure mode — the bond is a molecular interdiffusion, not a film of glue.

If your retort pack delaminates in the autoclave, the fix is almost never a better barrier resin. It is a better bond.

Designing a retort structure

  • PA or PP as the structural outer layer — PA for deep draw, PP for retort rigidity.
  • EVOH core sized with 30–50 % margin over the ambient barrier target.
  • Extruded tie layers, no solvent-based adhesives anywhere in the stack.
  • Seal layer formulated for the actual seal window of the line, not the theoretical one.

Validation is not optional

Every retort structure needs a real cycle on the actual product, on the actual line, at the actual fill. Accelerated shelf-life studies, dye-penetration leak tests and post-cycle OTR measurement all belong in the validation file. We support customer validation runs on site.

Cook-in and retort applications are where a competent barrier supplier earns their place. If you are qualifying a structure, talk to us before you buy the resin — the conversation is usually worth more than the material.