Ethylene vinyl alcohol copolymer — EVOH — is the highest-performing oxygen barrier polymer available for flexible packaging. It is not a compromise material and not a speciality niche. In a multilayer structure it does one job extraordinarily well: keeping oxygen out.
The chemistry in one paragraph
EVOH is a copolymer of ethylene and vinyl alcohol. The ethylene content determines almost everything. At 29 mol% vinyl content the barrier is superb but the melt is fragile. At 44 mol% the material is easy to process but the barrier weakens. Between those points sits the trade-off that every converter has to make.
What the barrier is actually worth
Measured at 23 °C and 65 % relative humidity, a 20 μm EVOH layer at 29 mol% passes roughly 0.2 cm³/m²·day of oxygen. That is aluminium-foil territory. The difference is flexibility: foil laminate cracks when your customer creases the pack or the product presses against a sharp edge in the carton.
EVOH is not a barrier on its own. It is a barrier layer inside a structure. The other layers decide how well it survives processing, storage and the customer's hands.
Where EVOH fails — and how to fix it
EVOH is hygroscopic. Above roughly 65 % relative humidity the absorbed water plasticises the polymer and the barrier collapses. This is not a defect; it is chemistry. Three things keep it in check: adequate gauge, a moisture barrier on either side, and conditioning of the resin before extrusion.
Practical guidance
- Never run EVOH below 60 % RH without conditioning the resin first.
- Specify a moisture barrier layer outside the EVOH core on both faces.
- For retort applications, validate 121 °C cycles — the barrier drops further during the heat exposure.
Choosing a grade
If you are converting on your own lines, 29 mol% gives you the strongest barrier and the most demanding processing. 32 mol% is the industrial compromise most converters settle on. 38 and 44 mol% exist for extrusion coating and pipe applications where melt strength matters more than barrier.
The honest summary: EVOH costs more per kilo than PA or PET and delivers a barrier nothing else in flexible packaging can match. Specify it where oxygen is the failure mode — lipid oxidation, aroma loss, chemical degradation — and leave it out where it is not.