A specification sheet is full of terms that sound obvious once you know them and mean nothing if you do not. This is the short version.

OTR — Oxygen Transmission Rate

The volume of oxygen passing through a film under a stated test condition, in cm³/m²·day. Lower is better. Always ask for the humidity: the same film at 0 % RH passes roughly ten times less oxygen than at 65 % RH.

WVTR — Water Vapour Transmission Rate

Mass of water passing through, in g/m²·day. Tested at 38 °C / 90 % RH for a realistic figure. This governs moisture pickup, not evaporation.

Tie layer

A thin coextruded layer that chemically bonds two otherwise incompatible polymers — PA to EVOH, EVOH to PE. It replaces adhesive. Adhesive laminates delaminate; tie layers do not.

Water quench

Cooling blown film in a chilled water bath rather than with air. The rapid quench produces finer crystallinity, giving higher clarity and better tear resistance.

Mono-material

A structure where every layer belongs to one recycling stream. PE/EVOH/PE qualifies. A structure containing PA plus metallised PET does not.

Gauge

Film thickness in microns. Watch the tolerance, not the nominal: 125 μm ± 7 % is a normal statement, 2 Sigma 2 % is a quality signal.

Seal window

The temperature range over which the seal holds. A narrow window — 120 to 130 °C — is a production risk on a line with normal temperature variation.

Peel force

Force required to remove a lidding film from its tray. Too low and it opens in transit; too high and the consumer cannot open it.

Form-fill-seal

A machine that forms a pouch from film, fills it and seals it in one pass. Film for FFS must be tuned for web tracking and walk-through performance, not just for barrier.

Retort

Heat processing at 121 °C for sterilisation. The barrier layer loses performance during the cycle, so retort structures are designed with margin rather than to the threshold.